Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tangent Modulus | 990 MPa | 144000 psi | ASTM D790 |
Flint Hills P5M6N-058A Polypropylene Random Copolymer Features: Excellent processabilty, nucleated and antistat. Product does not contain animal derived components. Phthalate-free.Applications: Injection Molding: consumer disposable itemsInformation .. |