Polymer Property : Tangent Modulus = 144000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tangent Modulus 990 MPa
144000 psi
ASTM D790
Flint Hills P5M6N-058A Polypropylene Random Copolymer
Features: Excellent processabilty, nucleated and antistat. Product does not contain animal derived components. Phthalate-free.Applications: Injection Molding: consumer disposable itemsInformation ..