Mechanical Properties | Metric | English | Comments |
---|---|---|---|
2% Secant Modulus | 0.0896 GPa | 13.0 ksi | |
3M Scotch® FP-301 Heat Shrink Tubing Scotch® Heat Shrink Tubing FP-301 offers an outstanding balance of electrical, physical and chemical properties for a wide variety of industrial and military applications. Rated for 135°C continuo.. |
|||
2% Secant Modulus | 0.0896 GPa | 13.0 ksi | |
3M Scotch® FP-301VW Heat Shrink Tubing Scotch® Heat Shrink Tubing FP-301VW has the same outstanding balance of electrical, physical and chemical properties as FP-301 tubing, and is specially engineered for excellent flame resistance. FP.. |