Mechanical Properties Metric English Comments
2% Secant Modulus 0.0896 GPa
13.0 ksi
3M Scotch® FP-301 Heat Shrink Tubing
Scotch® Heat Shrink Tubing FP-301 offers an outstanding balance of electrical, physical and chemical properties for a wide variety of industrial and military applications. Rated for 135°C continuo..
2% Secant Modulus 0.0896 GPa
13.0 ksi
3M Scotch® FP-301VW Heat Shrink Tubing
Scotch® Heat Shrink Tubing FP-301VW has the same outstanding balance of electrical, physical and chemical properties as FP-301 tubing, and is specially engineered for excellent flame resistance. FP..
Copyright © lookpolymers.com All Rights Reserved