Polymer Property : 2% Secant Modulus = 120 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
2% Secant Modulus 0.827 GPa
120 ksi
Crosshead speed - 0.5" min; ASTM D790
LyondellBasell Alathon® ETP H5057 High Density Polyethylene
ApplicationsALATHON H 5057 is a multi-purpose high-flow resin that exhibits enhanced low temperature impact performance, enhanced processability and thermal stability for fast cycling in multi-cavit..
2% Secant Modulus 0.827 GPa
120 ksi
ASTM D790
Ineos K44-15-186 Polyethylene Copolymer
K44-15-186 is a blue high-density polyethylene copolymer designed specifically for extrusion of pipe by blending K44-15-122 natural resin with G38-70C BLU II concentrate or an approved equivalent. ..