Crucible Steel S7 XL (Premium AISI S7) Tool Steel

Category Metal , Ferrous Metal , Tool Steel , Mold Steel
Manufacturer Crucible Steel
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Crucible Steel S7 XL (Premium AISI S7) Tool Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Crucible S7XL is a double refined, high purity grade of S7. The remelt operation produces a cleaner steel with a more uniform microstructure, offering the following advantages over conventional S7:Better Consistency in Wire EDM CuttingHigher Polishability for Critical Finish Plastic MoldsMore Uniform Texturing for Plastic MoldsHigher Transverse Impact Toughness (Across the Grain) Crucible S7 XL can be used in any application where AISI S7 is used.Information provided by Crucible Specialty Metals.
Physical Properties Metric English Comments
Density 7.83 g/cc
0.283 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 187 - 220
187 - 220
Annealed
Hardness, Rockwell C 57
57
Austenitizing Temperature- 955°C
Modulus of Elasticity 207 GPa
30000 ksi
Charpy Impact 125 J
92.2 ft-lb
Austenitizing Temperature- 955°C
Thermal Properties Metric English Comments
CTE, linear 12.6 µm/m-°C

@Temperature 20.0 - 205 °C
7.00 µin/in-°F

@Temperature 68.0 - 401 °F
13.7 µm/m-°C

@Temperature 20.0 - 540 °C
7.61 µin/in-°F

@Temperature 68.0 - 1000 °F
Thermal Conductivity 28.5 W/m-K

@Temperature 95.0 °C
198 BTU-in/hr-ft²-°F

@Temperature 203 °F
Component Elements Properties Metric English Comments
Carbon, C 0.55 %
0.55 %
Chromium, Cr 3.25 %
3.25 %
Iron, Fe 93.5 %
93.5 %
As Remainder
Manganese, Mn 0.70 %
0.70 %
Molybdenum, Mo 1.4 %
1.4 %
Silicon, Si 0.35 %
0.35 %
Vanadium, V 0.25 %
0.25 %