Mechanical Properties Metric English Comments
Charpy Impact >= 150 J
>= 111 ft-lb
Industeel CLC 18.10 Nb Niobium Stabilized 18Cr-10Ni Austenitic Stainless Steel
CLC 18-10Nb is a 18Cr-10Ni austenitic stainless steel stabilized with specific Nb addition. This kind of steel is one of the basic grades of the stainless steels range. Niobium bearing and its low c..
Charpy Impact >= 150 J
>= 111 ft-lb
Industeel CLC 18.10Ti Titanium-Stabilized 18Cr-10Ni Austenitic Stainless Steel
CLC 18-10Ti is a 18Cr-9Ni austenitic stainless steel stabilized with some Titanium additions. This is a basic grades in the stainless steel range. Titanium bearing (carbide forming element) avoids i..
Charpy Impact 150 J
111 ft-lb
Typical
Industeel URANUS® 35N 23.04 Duplex Stainless Steel with PREN = 24
Description: URANUS® 35N (UR 35N) is a 23% Cr, 4% Nickel, Mo free duplex stainless steel (23.04). The alloy UR 35N has similar corrosion resistance properties similar to 316L. Furthermore, its me..
Charpy Impact 150 J
111 ft-lb
ATI Allegheny Ludlum Stainless Steel Type 301, 3/4 Hard (UNS S30100)
Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho..
Charpy Impact 150 J

@Temperature -73.0 °C
111 ft-lb

@Temperature -99.4 °F
ATI Allegheny Ludlum Stainless Steel Type 301, 3/4 Hard (UNS S30100)
Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho..
Charpy Impact 150 J

@Temperature 196 °C
111 ft-lb

@Temperature 385 °F
ATI Allegheny Ludlum Stainless Steel Type 301, 3/4 Hard (UNS S30100)
Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho..
Charpy Impact 150 J
111 ft-lb
Typical
ATI Allegheny Ludlum AL 601™ Nickel-Base Alloy, Annealed at 982°C (1800°F), UNS N06601
Allegheny Ludlum's AL 601 alloy is an austenitic nickel-chromium-iron alloy designed for both heat and corrosion resistance. As compared to AL 600 alloy, the AL 601 alloy has, in addition to increa..
Charpy Impact 150 J
111 ft-lb
ATI Allegheny Ludlum Stainless Steel Type 301, 1/2 Hard (UNS S30100)
Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho..
Charpy Impact 150 J

@Temperature -73.0 °C
111 ft-lb

@Temperature -99.4 °F
ATI Allegheny Ludlum Stainless Steel Type 301, 1/2 Hard (UNS S30100)
Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho..
Charpy Impact 150 J

@Temperature 196 °C
111 ft-lb

@Temperature 385 °F
ATI Allegheny Ludlum Stainless Steel Type 301, 1/2 Hard (UNS S30100)
Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho..
Charpy Impact 150 J
111 ft-lb
ATI Allegheny Ludlum Stainless Steel Type 301, 1/4 Hard (UNS S30100)
Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho..
Charpy Impact 150 J

@Temperature -73.0 °C
111 ft-lb

@Temperature -99.4 °F
ATI Allegheny Ludlum Stainless Steel Type 301, 1/4 Hard (UNS S30100)
Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho..
Charpy Impact 150 J

@Temperature 196 °C
111 ft-lb

@Temperature 385 °F
ATI Allegheny Ludlum Stainless Steel Type 301, 1/4 Hard (UNS S30100)
Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho..
Charpy Impact 150 J
111 ft-lb
ATI Allegheny Ludlum Stainless Steel Type 301, annealed (UNS S30100)
Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho..
Charpy Impact 150 J

@Temperature -73.0 °C
111 ft-lb

@Temperature -99.4 °F
ATI Allegheny Ludlum Stainless Steel Type 301, annealed (UNS S30100)
Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho..
Charpy Impact 150 J

@Temperature 196 °C
111 ft-lb

@Temperature 385 °F
ATI Allegheny Ludlum Stainless Steel Type 301, annealed (UNS S30100)
Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho..
Charpy Impact 150 J
111 ft-lb
ATI Allegheny Ludlum Stainless Steel Type 301, Full Hard (UNS S30100)
Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho..
Charpy Impact 150 J

@Temperature -73.0 °C
111 ft-lb

@Temperature -99.4 °F
ATI Allegheny Ludlum Stainless Steel Type 301, Full Hard (UNS S30100)
Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho..
Charpy Impact 150 J

@Temperature 196 °C
111 ft-lb

@Temperature 385 °F
ATI Allegheny Ludlum Stainless Steel Type 301, Full Hard (UNS S30100)
Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho..
Charpy Impact 150 J
111 ft-lb
Typical
Industeel URANUS® 45N 22Cr 3Mo Duplex Stainless Steel with PREN = 33 or 34