Polymer Property : Modulus of Elasticity = 943 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 6.50 - 26.0 GPa
943 - 3770 ksi
Average value: 15.6 GPa Grade Count:24
Overview of materials for Polyarylamide, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyarylamide, Glass Fiber Filled". Each property range of values reported is minimum and maximum values..
Modulus of Elasticity 6.50 GPa
943 ksi
Lehmann & Voss LUVOCOM® 1301-8095 PPS, linear, with glass fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.High chemic..
Modulus of Elasticity 6.50 GPa
943 ksi
Lehmann & Voss LUVOCOM® 50-7289/V2 Polycarbonate, with carbon fiber and PTFE
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Electrically conductive, suitable for cont..
Modulus of Elasticity 6.50 GPa
943 ksi
Lehmann & Voss LUVOCOM® 50-7814/EM Polycarbonate, with glass fiber and PTFE
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi..
Modulus of Elasticity 6.50 GPa
943 ksi
Lehmann & Voss LUVOCOM® 80-8510 Polyacetal-copolymer, with mineral filler, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Modulus of Elasticity 6.50 GPa
943 ksi
Lehmann & Voss LUVOCOM® 50/GF/20/TF/20/GY Polycarbonate, with glass fiber and PTFE
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi..
Modulus of Elasticity 6.50 GPa
943 ksi
ISO 527
GEHR Plastics PP-30GF Polypropylene, 30% Glass Fiber
Polypropylene shows a high mechanical strength and a tensile strength, but a low notched impact strength. PP resists stress cracking and it is easy to weld. At minus temperatures it can get brittle...
Modulus of Elasticity 6.50 GPa
943 ksi
ISO 527-2
Tisan TISLAMID® 6 30% Glass Filled Impact Modified Nylon 6
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
Modulus of Elasticity 6.50 GPa
943 ksi
ISO 527-2
Tisan TISLAMID® 66 20% Glass Fiber Reinforced Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
Modulus of Elasticity 6.50 GPa
943 ksi
ISO 527-2
Tisan TISLAMID® 66 30% Glass Filled Impact Modified, Heat Stabilized Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
Modulus of Elasticity 6.50 GPa
943 ksi
ISO 178
Addiplast Addilene H 511 V30 Polypropylene Homopolymer
Glass fiber reinforced, high modulus and improved stiffnessInformation provided by Addiplast.
Modulus of Elasticity 6.50 GPa
943 ksi
Conditioned; ISO 178
Addiplast Addinyl A2H V25 Flame Retardant Nylon 66, 25% Glass Filled
Flame retardant, 25% glass fiber reinforced, with halogensInformation provided by Addiplast.
Modulus of Elasticity 6.50 GPa
943 ksi
ISO 527-1/-2
BASF Ultramid® A3EG5 25% Glass Filled PA66 (Conditioned)
Description: Glass fiber reinforced injection molding grade for machinery components and housings of high stiffness and dimensional stability such as coil formers and bearing cages. Also used for el..
Modulus of Elasticity 6.50 GPa
943 ksi
ISO 527
BASF Ultramid® A3WG5 25% Glass Filled PA66 (Conditioned)
Ultramid A3WG5 is a 25% glass fiber reinforced and heat resistance injection molding PA66 grade.
Modulus of Elasticity 6.50 - 9.50 GPa

@Temperature 120 - 160 °C
943 - 1380 ksi

@Temperature 248 - 320 °F
Average value: 8.00 GPa Grade Count:1
Overview of materials for Nylon 46, Flame Retarded + Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Flame Retarded + Glass Fiber Reinforced". Each property range of values reported is minimum an..
Modulus of Elasticity 6.50 GPa
943 ksi
ISO 527-1/-2
BASF Ultramid® B3UGM210 GR 22866 10/50% Glass/Mineral Filled PA6 FR (Conditioned)
Description: Halogen- and phosphorus-free injection-molding grade with very high rigidity, low smoke density and outstanding electrical properties.Information provided by BASF