Polymer Property : Modulus of Elasticity = 1380 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 6.50 - 9.50 GPa

@Temperature 120 - 160 °C
943 - 1380 ksi

@Temperature 248 - 320 °F
Average value: 8.00 GPa Grade Count:1
Overview of materials for Nylon 46, Flame Retarded + Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Flame Retarded + Glass Fiber Reinforced". Each property range of values reported is minimum an..
Modulus of Elasticity 1.50 - 9.50 GPa
218 - 1380 ksi
Average value: 4.46 GPa Grade Count:23
Overview of materials for Polypropylene, Glass Reinforced, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass Reinforced, Impact Modified". Each property range of values reported is minimum and..
Modulus of Elasticity 1.20 - 9.50 GPa
174 - 1380 ksi
Average value: 3.85 GPa Grade Count:28
Overview of materials for Nylon 6, MoS2 Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria..
Modulus of Elasticity 9.10 - 9.50 GPa

@Temperature 80.0 - 80.0 °C
1320 - 1380 ksi

@Temperature 176 - 176 °F
Average value: 9.40 GPa Grade Count:4
Overview of materials for Polypropylene with 60% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 60% Glass Fiber Filler". Specific grades with glass content between 55% and 64% are i..