Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 6.50 - 9.50 GPa @Temperature 120 - 160 °C |
943 - 1380 ksi @Temperature 248 - 320 °F |
Average value: 8.00 GPa Grade Count:1 |
Overview of materials for Nylon 46, Flame Retarded + Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Flame Retarded + Glass Fiber Reinforced". Each property range of values reported is minimum an.. |
|||
Modulus of Elasticity | 1.50 - 9.50 GPa | 218 - 1380 ksi | Average value: 4.46 GPa Grade Count:23 |
Overview of materials for Polypropylene, Glass Reinforced, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass Reinforced, Impact Modified". Each property range of values reported is minimum and.. |
|||
Modulus of Elasticity | 1.20 - 9.50 GPa | 174 - 1380 ksi | Average value: 3.85 GPa Grade Count:28 |
Overview of materials for Nylon 6, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Modulus of Elasticity | 9.10 - 9.50 GPa @Temperature 80.0 - 80.0 °C |
1320 - 1380 ksi @Temperature 176 - 176 °F |
Average value: 9.40 GPa Grade Count:4 |
Overview of materials for Polypropylene with 60% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 60% Glass Fiber Filler". Specific grades with glass content between 55% and 64% are i.. |