Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.300 - 0.550 GPa @Temperature 60.0 - 150 °C |
43.5 - 79.8 ksi @Temperature 140 - 302 °F |
Average value: 0.379 GPa Grade Count:1 |
Overview of materials for Nylon 6, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro.. |