Polymer Property : Modulus of Elasticity = 0.550 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.300 - 0.550 GPa

@Temperature 60.0 - 150 °C
43.5 - 79.8 ksi

@Temperature 140 - 302 °F
Average value: 0.379 GPa Grade Count:1
Overview of materials for Nylon 6, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro..