Polymer Property : Modulus of Elasticity = 0.300 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.300 - 1.30 GPa
43.5 - 189 ksi
Average value: 0.720 GPa Grade Count:75
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i..
Modulus of Elasticity 0.300 GPa
43.5 ksi
Lehmann & Voss LUVOCOM® 94-8485 LD-PE, unreinforced
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Reduced moment of inertia compared with metal parts.Dynamic stressed parts.Especially suitable ..
Modulus of Elasticity 0.300 GPa

@Temperature 23.0 °C
43.5 ksi

@Temperature 73.4 °F
MD/TD; ASTM D638
Mapal Plastics Maplon Type O Polypropylene Sheet
Properties: Corona treated on both sides for offset and screen printing, Extended shelf life, Low stress whitening, Suitable for die cuttingApplications: Stationery products, Offset printed item
Modulus of Elasticity 0.300 GPa

@Temperature 23.0 °C
43.5 ksi

@Temperature 73.4 °F
MD/TD; ASTM D638
Mapal Plastics Maplon Type S Polypropylene Sheet
Properties: Low stress whitening, Suitable for die cutting, Corona treated on both sides for offset and screen printingApplications: Stationery, Packaging, House-hold productsand printed items
Modulus of Elasticity 0.300 GPa
43.5 ksi
ASTM D638
ITW Plexus Plexusâ„¢ AO420FS Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.
Modulus of Elasticity 0.300 GPa
43.5 ksi
ISO R527
Arkema Group Orgalloy® LT 4060 ES Polyamide Alloy
Polyamide Alloy, Blow Molding of Technical PartsInformation provided by Arkema Group
Modulus of Elasticity 0.300 GPa
43.5 ksi
ISO R527
Arkema Group Orgalloy® LT 4060 Polyamide Alloy
Polyamide Alloy, Flexible gradeTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group
Modulus of Elasticity 0.300 - 0.550 GPa

@Temperature 60.0 - 150 °C
43.5 - 79.8 ksi

@Temperature 140 - 302 °F
Average value: 0.379 GPa Grade Count:1
Overview of materials for Nylon 6, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro..
Modulus of Elasticity 0.300 - 5.70 GPa

@Temperature 60.0 - 90.0 °C
43.5 - 827 ksi

@Temperature 140 - 194 °F
Average value: 1.26 GPa Grade Count:8
Overview of materials for Polypropylene, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of..
Modulus of Elasticity 0.300 GPa
43.5 ksi
ASTM D638
ITW Plexus Plexus™ MA440 Methacrylate Adhesive
Two-part, self-leveling adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.
Modulus of Elasticity 0.300 GPa
43.5 ksi
ISO 5527
Total Lacqtene® 1025 FH 24 LDPE blown film  (discontinued **)
Radical polyethylene made by high pressure tubular process. Slip and antiblock formulated grade for good transparent thin films. Advised temperature profile : 150 to 190°C.Information provided prov..