Polymer Property : Modulus of Elasticity = 725 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 3.00 - 5.00 GPa
435 - 725 ksi
Compression; ISO 527
Raschig Group DECAL® 5431 Phenolic
Organically and inorganically filled phenolic molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/..
Modulus of Elasticity 0.210 - 5.00 GPa
30.5 - 725 ksi
Average value: 2.55 GPa Grade Count:39
Overview of materials for Nylon 66/6
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb ..
Modulus of Elasticity 0.700 - 5.00 GPa
102 - 725 ksi
Average value: 2.51 GPa Grade Count:195
Overview of materials for Nylon 66, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..