Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.00 - 7.58 GPa | 290 - 1100 ksi | Average value: 4.70 GPa Grade Count:32 |
Overview of materials for Nylon 6, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Modulus of Elasticity | 2.65 - 7.58 GPa | 384 - 1100 ksi | Average value: 4.13 GPa Grade Count:16 |
Overview of materials for Polyimide, Graphite Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Graphite Filled". Each property range of values reported is minimum and maximum values of app.. |