Modulus of Elasticity 2.41 - 2.81 GPa

@Temperature 30.0 - 120 °C
350 - 408 ksi

@Temperature 86.0 - 248 °F
Average value: 1.78 GPa Grade Count:1
Overview of materials for Acetal Copolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of..
Modulus of Elasticity 2.41 - 2.81 GPa

@Thickness 1.50 - 4.00 mm
350 - 408 ksi

@Thickness 0.0591 - 0.157 in
Average value: 1.78 GPa Grade Count:1
Overview of materials for Acetal Copolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of..
Modulus of Elasticity 2.81 - 2.81 GPa

@Temperature -18.0 - -18.0 °C
408 - 408 ksi

@Temperature -0.400 - -0.400 °F
Average value: 2.81 GPa Grade Count:1
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma..