Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.41 - 2.81 GPa @Temperature 30.0 - 120 °C |
350 - 408 ksi @Temperature 86.0 - 248 °F |
Average value: 1.78 GPa Grade Count:1 |
Overview of materials for Acetal Copolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of.. |
|||
Modulus of Elasticity | 2.41 - 2.81 GPa @Thickness 1.50 - 4.00 mm |
350 - 408 ksi @Thickness 0.0591 - 0.157 in |
Average value: 1.78 GPa Grade Count:1 |
Overview of materials for Acetal Copolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of.. |
|||
Modulus of Elasticity | 2.81 - 2.81 GPa @Temperature -18.0 - -18.0 °C |
408 - 408 ksi @Temperature -0.400 - -0.400 °F |
Average value: 2.81 GPa Grade Count:1 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma.. |