Mechanical Properties Metric English Comments
Modulus of Elasticity 1.40 - 2.80 GPa
203 - 406 ksi
Average value: 2.10 GPa Grade Count:61
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is ..
Modulus of Elasticity 1.00 - 2.80 GPa
145 - 406 ksi
Average value: 1.86 GPa Grade Count:7
Overview of materials for Nylon 12, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Flame Retardant". Each property range of values reported is minimum and maximum values of appr..
Modulus of Elasticity 2.60 - 2.80 GPa
377 - 406 ksi
30-40% better than Nylon 6 with 4-5% loading
Süd-Chemie Nanofil® 9 Polymer Additive
Application:PS, PA 6, PA 6.6, PA-AlloysElectronicsElectrical PartsImproves: Mechanical Properties
Modulus of Elasticity 2.60 - 2.80 GPa
377 - 406 ksi
30-40% better than Nylon 6 with 4-5% loading
Süd-Chemie Nanofil® SE 3010 Polymer Additive
Application:PA 6, PA 6.6, PET, ABS, PS, PC-AlloysElectronicsElectrical PartsAutomotiveTechnical PartsImproves: Mechanical Properties, Melt Viscosity
Modulus of Elasticity 2.20 - 2.80 GPa
319 - 406 ksi
Average value: 2.54 GPa Grade Count:9
Overview of materials for Polyphenylene Ether + Styrene-Butadiene Blend