Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.280 GPa | 40.6 ksi | (stiffness), ASTM D882 |
DuPont™ Clysar® LE Polyolefin Shrink Packaging Film, 60 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat-shrinkable, multilayer film with the lowest shrink force available in the Clysar® line. Dupont Clysar® LES is .. |
|||
Modulus of Elasticity | 0.280 GPa | 40.6 ksi | (stiffness), ASTM D882 |
DuPont™ Clysar® LE Polyolefin Shrink Packaging Film, 75 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat-shrinkable, multilayer film with the lowest shrink force available in the Clysar® line. Dupont Clysar® LES is .. |
|||
Modulus of Elasticity | 0.280 GPa @Temperature 23.0 °C |
40.6 ksi @Temperature 73.4 °F |
MD/TD; ASTM D638 |
Mapal Plastics Maplon Type 3G Polypropylene Sheet Maplon type “3G†is a single layer highly polished clear sheets, with anti-blocking properties.Main advantages: High clarity and low haze, Easy to convert due to reduced blocking, High dur.. |
|||
Modulus of Elasticity | 0.280 GPa @Temperature 23.0 °C |
40.6 ksi @Temperature 73.4 °F |
MD/TD; ASTM D638 |
Mapal Plastics Maplon Type D Polypropylene Sheet Main advantages: High clarity and medium haze, High durability, Water and chemical resistance, High heat resistance, Unlimited flex life of integral hinge, Easy to convertMain disadvantages: Low scr.. |
|||
Modulus of Elasticity | 0.280 GPa | 40.6 ksi | |
BASF Elastollan® 1164D Polyether Type Polyurethane Elastomer Recommended for injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes. They exhi.. |
|||
Modulus of Elasticity | 0.280 - 2.05 GPa | 40.6 - 297 ksi | Average value: 0.710 GPa Grade Count:12 |
Overview of materials for Polypropylene, Sheet/Thermoforming Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Sheet/Thermoforming Grade". Each property range of values reported is minimum and maximum.. |