Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Modulus of Elasticity = 0.280 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.280 GPa
40.6 ksi
(stiffness), ASTM D882
DuPont™ Clysar® LE Polyolefin Shrink Packaging Film, 60 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat-shrinkable, multilayer film with the lowest shrink force available in the Clysar® line. Dupont Clysar® LES is ..
Modulus of Elasticity 0.280 GPa
40.6 ksi
(stiffness), ASTM D882
DuPont™ Clysar® LE Polyolefin Shrink Packaging Film, 75 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat-shrinkable, multilayer film with the lowest shrink force available in the Clysar® line. Dupont Clysar® LES is ..
Modulus of Elasticity 0.280 GPa

@Temperature 23.0 °C
40.6 ksi

@Temperature 73.4 °F
MD/TD; ASTM D638
Mapal Plastics Maplon Type 3G Polypropylene Sheet
Maplon type “3G” is a single layer highly polished clear sheets, with anti-blocking properties.Main advantages: High clarity and low haze, Easy to convert due to reduced blocking, High dur..
Modulus of Elasticity 0.280 GPa

@Temperature 23.0 °C
40.6 ksi

@Temperature 73.4 °F
MD/TD; ASTM D638
Mapal Plastics Maplon Type D Polypropylene Sheet
Main advantages: High clarity and medium haze, High durability, Water and chemical resistance, High heat resistance, Unlimited flex life of integral hinge, Easy to convertMain disadvantages: Low scr..
Modulus of Elasticity 0.280 GPa
40.6 ksi
BASF Elastollan® 1164D Polyether Type Polyurethane Elastomer
Recommended for injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes. They exhi..
Modulus of Elasticity 0.280 - 2.05 GPa
40.6 - 297 ksi
Average value: 0.710 GPa Grade Count:12
Overview of materials for Polypropylene, Sheet/Thermoforming Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Sheet/Thermoforming Grade". Each property range of values reported is minimum and maximum..