Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 1.50 - 2.60 GPa @Temperature -18.0 - 71.0 °C |
218 - 377 ksi @Temperature -0.400 - 160 °F |
Average value: 2.05 GPa Grade Count:1 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and .. |
|||
Modulus of Elasticity | 2.00 - 2.60 GPa | 290 - 377 ksi | Average value: 2.35 GPa Grade Count:63 |
Overview of materials for Polycarbonate, UV Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a.. |
|||
Modulus of Elasticity | 1.72 - 2.60 GPa | 250 - 377 ksi | Average value: 2.18 GPa Grade Count:25 |
Overview of materials for Acrylic/Polycarbonate Alloy This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy". Each property range of values reported is minimum and maximum values of ap.. |
|||
Modulus of Elasticity | 1.70 - 2.60 GPa | 247 - 377 ksi | Average value: 2.26 GPa Grade Count:5 |
Overview of materials for Acrylic, Impact Modified Sheet This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified Sheet". Each property range of values reported is minimum and maximum values of.. |