Polymer Property : Modulus of Elasticity = 320 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 320 GPa
46400 ksi
H.C. Starck HPM 1700 Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
Modulus of Elasticity 320 GPa
46400 ksi
H.C. Starck HPM 1710 Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
Modulus of Elasticity 320 GPa
46400 ksi
ASTM-F417
CeramTec Alunit® Aluminum Nitride
Alunit® offers an extremely high thermal conductivity of 180 W/mK and outstanding electrical insulation properties. The thermal expansion coefficient of this material is comparable to silicon. Its ..
Modulus of Elasticity 320 GPa
46400 ksi
ASTM-F417
CeramTec Alunit® HS Aluminum Nitride
Alunit® HS offers an extremely high thermal conductivity of 170 W/mK and outstanding electrical insulation properties. The thermal expansion coefficient of this material is comparable to silicon. I..
Modulus of Elasticity 320 GPa
46400 ksi
CeramTec Rubalit® A 1894 Alumina, 94%
Rubalit® A 1894 (94%) was specifically developed in response to electrical and electronic engineering needs. In conjunction with CeramTec's complementary metallization systems, a vacuum-tight bond ..
Modulus of Elasticity 320 GPa
46400 ksi
Tokuyama Shapal™ SH-50 Sintered Aluminum Nitride
Uniform, large sized pressed sintered aluminum nitride.
Modulus of Elasticity 320 GPa
46400 ksi
Zircar Refractory Composites RSMAT-3000 ALUMINA MAT
ZRCI Type RSMAT-3000 is a high purity, high temperature, flexible form composed of continuous 97% alumina ceramic fibers designed for use to 1650°C (3002°F). Type RSMAT-3000 contains little shot a..
Modulus of Elasticity 320 GPa
46400 ksi
Zircar Ceramics Alumina Mat
A layered, low density flexible mat made of 100% polycrystalline alumina fiber (non-RCF) designed for use to temperatures as high as 1650°C (3002°F). Shot free low density mat used as fill between..
Modulus of Elasticity 320 GPa
46400 ksi
Ceradyne Ceralloy® 1370-1E Aluminum Nitride
Features:standard grade Applications:semiconductor componentsInformation provided by Ceradyne Company
Modulus of Elasticity 320 GPa
46400 ksi
Ceradyne Ceralloy® 1370CS Aluminum Nitride
Features:high thermal conductivityApplications:semiconductor componentsInformation provided by Ceradyne Company
Modulus of Elasticity 320 GPa
46400 ksi
Ceradyne Ceralloy® 1370DP Aluminum Nitride
Features:high thermal conductivityApplications:semiconductor componentsmicrowave componentsInformation provided by Ceradyne Company
Modulus of Elasticity 320 GPa
46400 ksi
Ceradyne Ceralloy® 147-5 Silicon Nitride
Ceralloy® 147 Hot Pressed Silicon Nitride (HPSN) can be formulated into a variety of compositions having minimal densification aids. These HPSN compositions offer the highest strength of Ceradyne's..
Modulus of Elasticity 320 GPa
46400 ksi
Advanced Ceramics ACL 1085 (C-795) Alumina
Information provided by Advanced Ceramics Limited (ACL)
Modulus of Elasticity 320 GPa
46400 ksi
ASTM-F417
CeramTec CeramCool® Alunit® Aluminum Nitride
CeramCool® is a metallized ceramic heat-sink for high power applications demonstrated by high power LED-systems. CeramCool® material characteristics: electrical insulation, high volume resistivit..