Ceradyne Ceralloy® 1370CS Aluminum Nitride

Category Ceramic , Nitride
Manufacturer Ceradyne Advanced Ceramics
Trade Name Ceralloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ceradyne Ceralloy® 1370CS Aluminum Nitride.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features:high thermal conductivityApplications:semiconductor componentsInformation provided by Ceradyne Company
Physical Properties Metric English Comments
Density 3.30 g/cc
0.119 lb/in³
Weibull Modulus 37
37
Mechanical Properties Metric English Comments
Vickers Microhardness 1000
1000
Modulus of Elasticity 320 GPa
46400 ksi
Flexural Strength 200 MPa

@Temperature 23.0 °C
29000 psi

@Temperature 73.4 °F
Poissons Ratio 0.24
0.24
Fracture Toughness 3.00 MPa-m½
2.73 ksi-in½
Shear Modulus 129 GPa
18700 ksi
calculated
Thermal Properties Metric English Comments
CTE, linear 5.60 µm/m-°C

@Temperature 20.0 - 1000 °C
3.11 µin/in-°F

@Temperature 68.0 - 1830 °F
Thermal Conductivity 170 W/m-K
1180 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
Dielectric Constant 8.9
8.9
Descriptive Properties Value Comments
Grain Size, microns 10
Purity, % 99