Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.07 - 3.21 GPa | 300 - 466 ksi | Average value: 2.60 GPa Grade Count:10 |
Overview of materials for Acetal Copolymer, Silicone Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Silicone Filled". Each property range of values reported is minimum and maximum values.. |
|||
Modulus of Elasticity | 2.07 - 25.5 GPa | 300 - 3700 ksi | Average value: 10.9 GPa Grade Count:94 |
Overview of materials for Polycarbonate, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v.. |
|||
Modulus of Elasticity | 2.07 - 15.9 GPa | 300 - 2300 ksi | Average value: 4.16 GPa Grade Count:11 |
Overview of materials for Polycarbonate, Conductive This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Conductive". Each property range of values reported is minimum and maximum values of appr.. |
|||
Modulus of Elasticity | 2.07 GPa | 300 ksi | ASTM D638 |
Ex-Tech Plastics PerformaTech™ PVC Ex-Alloy 200 Reprocessed Vinyl Ex-Tech Plastics has long been a market leader in reprocessing vinyl sheet used for a variety of high quality thermoformed packaging. From retail packaging to tri-folds to trays to blister and clams.. |
|||
Modulus of Elasticity | 2.07 GPa | 300 ksi | 2.0 in/min; ASTM D638 |
Ineos Nova Zyntar® 7041 High Performance Flame Retardant Polystyrene
(discontinued **) Non-Decabromodiphenyl Oxide, High flow, Ease of processingApplications: Electronics, TelevisionsThis is an impact grade of polystyrene containing chemicals to increase resistance to ignition in labo.. |