Polymer Property : Modulus of Elasticity = 15.9 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 2.07 - 15.9 GPa
300 - 2300 ksi
Average value: 4.16 GPa Grade Count:11
Overview of materials for Polycarbonate, Conductive
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Conductive". Each property range of values reported is minimum and maximum values of appr..
Modulus of Elasticity 1.31 - 15.9 GPa
190 - 2300 ksi
Average value: 9.89 GPa Grade Count:162
Overview of materials for Nylon 6, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E..
Modulus of Elasticity 0.965 - 15.9 GPa
140 - 2300 ksi
Average value: 3.01 GPa Grade Count:75
Overview of materials for Acetal Copolymer, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of ..