Modulus of Elasticity 8.50 - 22.0 GPa
1230 - 3190 ksi
Average value: 12.6 GPa Grade Count:21
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max..
Modulus of Elasticity 8.00 - 22.0 GPa

@Temperature 60.0 - 150 °C
1160 - 3190 ksi

@Temperature 140 - 302 °F
Average value: 15.1 GPa Grade Count:3
Overview of materials for Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled". Each property range of values reported is mini..