Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 215 GPa @Temperature 100 °C |
31200 ksi @Temperature 212 °F |
|
Outokumpu 4016 Ferritic Stainless Steel Fairly good corrosion resistant formable steel in mildly corrosive environments. Oxidation resistant at elevated temperatures (up to ~800°C). Ductile, does not work harden readily, and is well su.. |
|||
Modulus of Elasticity | 215 GPa | 31200 ksi | RT |
Outokumpu 4021 Martensitic Stainless Steel Moderate corrosion resistant stainless steel hardenable up to 1000N/mm2. Re-sulphurized steel improves machining properties.Applications: ShaftsKnivesFastenersSurgical applicationsDomestic applicat.. |
|||
Modulus of Elasticity | 215 GPa | 31200 ksi | RT |
Outokumpu 4028 Martensitic Stainless Steel Moderate corrosion resistant stainless steel hardenable up to 1000N/mm2. Re-sulphurized steel improves machining properties.Applications: ShaftsKnivesFastenersSurgical applicationsDomestic applicat.. |
|||
Modulus of Elasticity | 215 GPa | 31200 ksi | |
Crucible Steel CPM® S90V® (420V®) Tool Steel CPM S90V is a unique tool steel made by the Crucible Particle Metallurgy process. It is a martensitic stainless steel with a high volume of vanadium carbides for exceptionally good wear resistance. .. |
|||
Modulus of Elasticity | 215 GPa | 31200 ksi | 68°F, (hardened and tempered to 350 HB) |
Bohler-Uddeholm BÖHLER RAMAX® HH Modified 420F Chromium alloyed steelTypical applications for Ramax® HH are: holders and bolsters for plastic molds, plastic and rubber molds with low requirements on polishability, and dies for plastic extrusion.. |
|||
Modulus of Elasticity | 215 GPa | 31200 ksi | (hardness of 40 HRC) |
Bohler-Uddeholm UDDEHOLM ALVAR 14 Hot Work Tool Steel Alvar 14 is a chromium-nickel-molybdenumvanadium alloyed steel ALVAR 14 is characterized by: Good toughnessGood resistance to high thermal stresses Good stability in hardeningGood through-hardening.. |