Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.01957 GPa | 2.838 ksi | ASTM E 831 |
Arlon R36580N008 0.008" ((0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassAppearance: Grey silicone gumThis data represents typical values for the production material. The dat.. |
|||
Modulus of Elasticity | 0.01957 GPa | 2.838 ksi | ASTM E 831 |
Arlon R36580N015 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassAppearance: Grey silicone gumThis data represents typical values for the production material. The dat.. |
|||
Modulus of Elasticity | 0.01957 GPa | 2.838 ksi | silicone property; Arlon SQA-TMS-008 |
Arlon Thermabond® 99950N008 Silicone Rubber/Fiberglass Laminate Electrically conductive, Thermabond®. primerless. Liner: 1 mil FEP; Product: uncured silicone rubber; Carrier: 3 mil PTFE coated fiberglass. |
|||
Modulus of Elasticity | 0.01957 GPa | 2.838 ksi | silicone property; Arlon SQA-TMS-008 |
Arlon Thermabond® 99950N015 Silicone Rubber/Fiberglass Laminate Electrically conductive, Thermabond®. primerless. Liner: 1 mil FEP; Product: uncured silicone rubber; Carrier: 3 mil PTFE coated fiberglass. |