Polymer Property : Modulus of Elasticity = 0.01957 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.01957 GPa
2.838 ksi
ASTM E 831
Arlon R36580N008 0.008" ((0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass
Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassAppearance: Grey silicone gumThis data represents typical values for the production material. The dat..
Modulus of Elasticity 0.01957 GPa
2.838 ksi
ASTM E 831
Arlon R36580N015 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassAppearance: Grey silicone gumThis data represents typical values for the production material. The dat..
Modulus of Elasticity 0.01957 GPa
2.838 ksi
silicone property; Arlon SQA-TMS-008
Arlon Thermabond® 99950N008 Silicone Rubber/Fiberglass Laminate
Electrically conductive, Thermabond®. primerless. Liner: 1 mil FEP; Product: uncured silicone rubber; Carrier: 3 mil PTFE coated fiberglass.
Modulus of Elasticity 0.01957 GPa
2.838 ksi
silicone property; Arlon SQA-TMS-008
Arlon Thermabond® 99950N015 Silicone Rubber/Fiberglass Laminate
Electrically conductive, Thermabond®. primerless. Liner: 1 mil FEP; Product: uncured silicone rubber; Carrier: 3 mil PTFE coated fiberglass.