Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lehmann & Voss LUVOCOM® 21-8115 Polyamide 6/6T, with carbon fiber, lubricant modified

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Carbon Fiber Filled
Manufacturer Lehmann & Voss & Co.
Trade Name LUVOCOM®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lehmann & Voss LUVOCOM® 21-8115 Polyamide 6/6T, with carbon fiber, lubricant modified.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear behaviour. Emergency running property.Bearings, sleeves, control disks, gear wheels, pump impellers, gear parts.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.45 g/cc
1.45 g/cc
ISO 1183
Water Absorption <= 0.30 %
<= 0.30 %
23°C/24h
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
Mechanical Properties Metric English Comments
Tensile Stress 150 MPa
21800 psi
Elongation at Yield 1.4 %
1.4 %
1.8 %
1.8 %
flexural
Modulus of Elasticity 13.0 GPa
1890 ksi
Flexural Strength 215 MPa
31200 psi
Flexural Modulus 11.0 GPa
1600 ksi
Charpy Impact Unnotched 2.10 J/cm²
9.99 ft-lb/in²
edgewise; ISO 179 1eU
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 135 °C
275 °F
160 °C
320 °F
short term
Electrical Properties Metric English Comments
Surface Resistance <= 1.00e+9 ohm
<= 1.00e+9 ohm
Insulation Resistance <= 1.00e+9 ohm
<= 1.00e+9 ohm
Processing Properties Metric English Comments
Processing Temperature 330 °C
626 °F
mass temp
Nozzle Temperature 330 - 340 °C
626 - 644 °F
Zone 1 300 - 340 °C
572 - 644 °F
Zone 2 310 - 340 °C
590 - 644 °F
Zone 3 320 - 340 °C
608 - 644 °F
Mold Temperature 90.0 - 120 °C
194 - 248 °F
Drying Temperature 80.0 °C

@Time 21600 - 57600 sec
176 °F

@Time 6.00 - 16.0 hour
Dehumidifying dryer
110 °C

@Time 14400 - 21600 sec
230 °F

@Time 4.00 - 6.00 hour
or
Descriptive Properties Value Comments
Color natural color (black)