Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 10.3 - 29.0 GPa | 1490 - 4210 ksi | Average value: 15.2 GPa Grade Count:8 |
Overview of materials for Phenolic, Novolac, Mineral/Graphite Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Graphite Filled". Each property range of values reported is minimum and maxim.. |
|||
Modulus of Elasticity | 10.3 GPa | 1490 ksi | ISO 527 |
GEHR Plastics PEEK-30GF Polyetheretherketone, 30% Glass Fiber Polyether etherketone can be used at very high temperatures and it shows a good mechanical strength, toughness, hardness, flexural strength, and torsional strength. PEEK exhibits excellent chemical .. |