Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 13.5 - 15.0 GPa @Temperature 70.0 - 70.0 °C |
1960 - 2180 ksi @Temperature 158 - 158 °F |
Average value: 10.1 GPa Grade Count:1 |
Overview of materials for Nylon 6, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E.. |
|||
Modulus of Elasticity | 13.5 - 15.0 GPa @Time 180000 - 1.44e+6 sec |
1960 - 2180 ksi @Time 50.0 - 400 hour |
Average value: 10.1 GPa Grade Count:1 |
Overview of materials for Nylon 6, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E.. |
|||
Modulus of Elasticity | 13.5 GPa | 1960 ksi | |
Lehmann & Voss LUVOTECH® GS 58 Polyamide 66, with glass fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |