Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 80.0 GPa | 11600 ksi | |
Osprey Metals CE17 Al-Si Controlled Expansion Alloy Al-27%Si controlled expansion alloy manufactured and patented by Osprey Metals Ltd.Information provided to MatWeb by Osprey Metals. |
|||
Modulus of Elasticity | >= 80.0 GPa | >= 11600 ksi | |
PEAK Werkstoff DISPAL S220 Aluminum Alloy, AlSi35, Condition O Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
Modulus of Elasticity | >= 80.0 GPa @Temperature 150 °C |
>= 11600 ksi @Temperature 302 °F |
Condition T6x (Quench in water at RT) |
PEAK Werkstoff DISPAL S232 Aluminum Alloy, AlSi17Fe4Cu3Mg, Condition T6 Heat Treatment Condition T6 (Quench in water at RT). Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allo.. |
|||
Modulus of Elasticity | >= 80.0 GPa @Temperature 150 °C |
>= 11600 ksi @Temperature 302 °F |
|
PEAK Werkstoff DISPAL S232 Aluminum Alloy, AlSi17Fe4Cu3Mg, Condition T6x Heat Treatment Condition T6x (Quench in water at RT). Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials all.. |
|||
Modulus of Elasticity | 79.7 GPa | 11600 ksi | parallel to c-axis |
Mateck Magnesium Fluoride (MgF2) Optical crystals |
|||
Modulus of Elasticity | 80.0 GPa | 11600 ksi | |
Schott LAFN7 Glass Information Provided by SCHOTT North America, Inc. |
|||
Modulus of Elasticity | 80.0 GPa | 11600 ksi | |
Sapco C 220 Steatite Information provided by Sapco. |
|||
Modulus of Elasticity | 80.0 GPa | 11600 ksi | |
AGY ADVANTEX® Generic Glass Fiber OC/AGY E-CR glass. Various silanes and starch oil are used as binders. Acid resistant. Lower alkali resistance than VeTron® and ZenTron® glass fibers.Information provided by AGY Holding Corp... |