Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.0130 - 10.5 GPa | 1.89 - 1520 ksi | Average value: 0.426 GPa Grade Count:68 |
Overview of materials for Polyester Thermoplastic Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values.. |
|||
Modulus of Elasticity | 3.80 - 10.5 GPa | 551 - 1520 ksi | Average value: 7.73 GPa Grade Count:38 |
Overview of materials for Polycarbonate, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E.. |