Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.276 - 0.703 GPa | 40.0 - 102 ksi | ASTM D638M |
DSM Somos® 8120 Epoxy Photopolymer
(discontinued **) DescriptionDSM Somos® 8120 is a high-speed liquid photopolymer that produces flexible, high-impact-strength, accurate parts using stereolithography machines. It has a wide processing latitude and .. |