Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Modulus of Elasticity = 102 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.0110 - 0.700 GPa
1.60 - 102 ksi
Average value: 0.0939 GPa Grade Count:21
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate; Molded/Extruded". Each property range of values reported is minimum and maximum ..
Modulus of Elasticity 0.276 - 0.703 GPa
40.0 - 102 ksi
ASTM D638M
DSM Somos® 8120 Epoxy Photopolymer  (discontinued **)
DescriptionDSM Somos® 8120 is a high-speed liquid photopolymer that produces flexible, high-impact-strength, accurate parts using stereolithography machines. It has a wide processing latitude and ..
Modulus of Elasticity 0.276 - 0.700 GPa
40.0 - 102 ksi
Average value: 0.454 GPa Grade Count:8
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyperfluoroalkoxyethylene, Molded/Extruded". Each property range of values reported is minimum and max..
Modulus of Elasticity 0.343 - 0.700 GPa
49.7 - 102 ksi
Average value: 0.378 GPa Grade Count:11
Overview of materials for Fluorinated Ethylene Propylene (FEP), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Fluorinated Ethylene Propylene (FEP), Molded/Extruded". Each property range of values reported is minimu..
Copyright © lookpolymers.com All Rights Reserved