Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.297 GPa | 43.1 ksi | Secant; ASTM D638 |
Huntsman PE1065 Film Extrusion Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Yields film with excellent optical and machinability.Applications: Film extrusion: soft goods and other high clarity packaging.FDA Notes: Conforms to FDA regu.. |
|||
Modulus of Elasticity | 0.297 GPa | 43.1 ksi | Secant; ASTM D638 |
Huntsman PE1059 Film Extrusion Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Excellent draw down and good processability.Applications: Film extrusion: non-abrasive packaging applications.FDA Notes: Conforms to FDA regulation 21 CFR 177.. |
|||
Modulus of Elasticity | 0.297 GPa | 43.1 ksi | Secant; ASTM D638 |
Huntsman PE8020 Specialty Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Yields film with excellent draw down and machinability.Applications: Film extrusion: gel free film applications.FDA Notes: Conforms to FDA regulation 21 CFR 1.. |