Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Modulus of Elasticity = 1.90 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.0689 - 1.90 GPa
10.0 - 275 ksi
Average value: 0.579 GPa Grade Count:25
Overview of materials for Methacrylate Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Methacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropri..
Modulus of Elasticity 0.500 - 1.90 GPa

@Temperature 60.0 - 90.0 °C
72.5 - 276 ksi

@Temperature 140 - 194 °F
Average value: 1.78 GPa Grade Count:8
Overview of materials for Acetal Copolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of..
Modulus of Elasticity 1.50 - 1.90 GPa

@Temperature 60.0 - 90.0 °C
218 - 276 ksi

@Temperature 140 - 194 °F
Average value: 1.70 GPa Grade Count:1
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep..
Modulus of Elasticity 0.000517 - 1.90 GPa
0.0750 - 276 ksi
Average value: 0.0881 GPa Grade Count:27
Overview of materials for Silicone Rubber
This property data is a summary of similar materials in the MatWeb database for the category "Silicone Rubber". Each property range of values reported is minimum and maximum values of appropriate Ma..
Modulus of Elasticity 0.350 - 1.90 GPa

@Temperature 60.0 - 150 °C
50.8 - 276 ksi

@Temperature 140 - 302 °F
Average value: 0.850 GPa Grade Count:1
Overview of materials for Nylon 66, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Modulus of Elasticity 0.00260 - 1.90 GPa
0.377 - 276 ksi
Average value: 0.818 GPa Grade Count:8
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyester Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyester Grade". Each property range of values reported is minimum a..
Modulus of Elasticity 1.10 - 1.90 GPa
160 - 276 ksi
Average value: 1.64 GPa Grade Count:9
Overview of materials for Polypropylene with 10% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Mica Filler". Specific grades with primary filler content between 5% and 14% are ..
Copyright © lookpolymers.com All Rights Reserved