Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1 hour | 6100 MPa | 885000 psi | ISO 899-1 |
Lanxess Durethan® BKV 140 000000 Copolyamide, 40% Glass Fiber CoPA, injection molding grade, 40% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 40, even in.. |
|||
Tensile Creep Modulus, 1 hour | 6100 MPa | 885000 psi | ISO 899-1 |
Lanxess Durethan® BKV 140 H2.0 900051 Copolyamide, 40% Glass Fiber CoPA, injection molding grade, 40% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 40, even in.. |
|||
Tensile Creep Modulus, 1 hour | 6100 MPa | 885000 psi | |
BASF Luranyl® KR 2403 G4 Polyphenylene Ether + Styrene-Butadiene Blend, 20% Glass Fiber Reinforced General-purpose grade with 20% glass fiber for parts requiring especially good resistance to heat deformation.Applications: sanitary fittings and parts for fans, computer keyboards.Data was collecte.. |