Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Creep Modulus, 1 hour = 2600 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1 hour 2600 MPa

@Temperature 23.0 °C
377000 psi

@Temperature 73.4 °F
ISO 899
DuPont Performance Polymers Crastin® FG6129 NC010 PBT  (Unverified Data**)
Crastin® FG6129 NC010 is an unreinforced, high viscosity polybutylene terephthalate resin for extrusion and injection molding. It has been developed for consideration into applications such as part..
Tensile Creep Modulus, 1 hour 2600 MPa

@Temperature 23.0 °C
377000 psi

@Temperature 73.4 °F
ISO 899
DuPont Performance Polymers Crastin® S600F20 NC010 PBT  (Unverified Data**)
Crastin® S600F20 NC010 is an unreinforced, lubricated, medium viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Creep Modulus, 1 hour 2600 MPa

@Temperature 23.0 °C
377000 psi

@Temperature 73.4 °F
ISO 899
DuPont Performance Polymers Crastin® S600F40 NC010 PBT  (Unverified Data**)
Crastin® S600F40 NC010 is an unreinforced, lubricated, low viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Creep Modulus, 1 hour 2600 MPa
377000 psi
Arkema Group Oroglas® MI-2T Acrylic  (discontinued **)
OROGLAS MI-2T is an injection molding acrylic grade that offers excellent thermal resistance with slight improvement in impact performance.Key features improved deformation and toughness : up to 2..
Tensile Creep Modulus, 1 hour 2600 MPa
377000 psi
ISO 899-1
Lanxess Durethan® BKV 115 H2.0 901510 Copolyamide, 15% Glass Fiber
CoPA, injection molding grade, 15% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 15, even in..
Tensile Creep Modulus, 1 hour 2600 MPa
377000 psi
ISO 899-1
Lanxess Durethan® BKV 115 000000 Copolyamide, 15% Glass Fiber
CoPA, injection molding grade, 15% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 15, even in..
Tensile Creep Modulus, 1 hour 2600 MPa

@Time 3600 sec
377000 psi

@Time 1.00 hour
ISO 899-1
DuPont Performance Polymers Crastin® FG6129 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)<
Unreinforced High Viscosity Polybutylene Terephthalate Developed for Food Contact Applications and Extrusion and Injection Molding Crastin FG6129 NC010 is an unreinforced high viscosity polybutylene..
Tensile Creep Modulus, 1 hour 2600 MPa

@Time 3600 sec
377000 psi

@Time 1.00 hour
ISO 899-1
DuPont Performance Polymers Crastin® FGS600F10 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
Unreinforced Polybutylene Terephthalate Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Creep Modulus, 1 hour 2600 MPa

@Time 3600 sec
377000 psi

@Time 1.00 hour
ISO 899-1
DuPont Performance Polymers Crastin® FGS600F40 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
Unreinforced Low Viscosity Polybutylene Terephthalate Developed for Food Contact Applications Crastin FGS600F40 NC010 is an unreinforced low viscosity polybutylene terephthalate resin for injection ..
Tensile Creep Modulus, 1 hour 2600 MPa

@Time 3600 sec
377000 psi

@Time 1.00 hour
ISO 899-1
DuPont Performance Polymers Crastin® S600F40 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
Unreinforced Low Viscosity Polybutylene Terephthalate Crastin S600F40 NC010 is an unreinforced lubricated low viscosity polybutylene terephthalate resin for injection molding.Information provided by..
Tensile Creep Modulus, 1 hour 2600 MPa

@Time 3600 sec
377000 psi

@Time 1.00 hour
ISO 899-1
DuPont Performance Polymers Crastin® S620F20 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
Unreinforced Medium Viscosity Polybutylene Terephthalate Crastin S620F20 NC010 is an unreinforced nucleated lubricated medium viscosity polybutylene terephthalate resin for fast injection molding.In..
Tensile Creep Modulus, 1 hour 2600 MPa
377000 psi
Arkema Group Oroglas® V 045 I Acrylic, Extrusion Grade  (discontinued **)
OROGLAS V 045 I is an extrusion that exhibits the following properties : 50% tougher than standard acrylics excellent optical properties ( comparable to that of standard acrylics) superior surface ..
Tensile Creep Modulus, 1 hour 2600 MPa
377000 psi
Arkema Group Oroglas® VM Acrylic, Injection Molding Grade  (discontinued **)
OROGLAS VM is an injection molding grade with a medium heat resistance and easy flow.OROGLAS VM is particularly suitable to improve mold filling of technical parts.The VM L version has been speciall..
Copyright © lookpolymers.com All Rights Reserved