Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 98.1 - 358 kJ/m² | 46.7 - 170 ft-lb/in² | Average value: 167 kJ/m² Grade Count:5 |
Overview of materials for Acetal Homopolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values .. |
|||
Tensile Impact Strength | 98.1 kJ/m² | 46.7 ft-lb/in² | 0.0630 in; ASTM D1822 |
KEP Kepital® F40 Standard Grade/Low Viscosity Acetal Homopolymer injection molding: electrical parts, machine/mechanical parts, industrial parts, automotive applications, electronic data processing.Kepital® is a registered trademark of Korea Engineering Plasti.. |