Mechanical Properties Metric English Comments
Tensile Impact Strength 98.1 - 358 kJ/m²
46.7 - 170 ft-lb/in²
Average value: 167 kJ/m² Grade Count:5
Overview of materials for Acetal Homopolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values ..
Tensile Impact Strength 98.1 kJ/m²
46.7 ft-lb/in²
0.0630 in; ASTM D1822
KEP Kepital® F40 Standard Grade/Low Viscosity Acetal Homopolymer
injection molding: electrical parts, machine/mechanical parts, industrial parts, automotive applications, electronic data processing.Kepital® is a registered trademark of Korea Engineering Plasti..