Polymer Property : Tensile Impact Strength = 170 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Impact Strength 98.1 - 358 kJ/m²
46.7 - 170 ft-lb/in²
Average value: 167 kJ/m² Grade Count:5
Overview of materials for Acetal Homopolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values ..