Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 137 kJ/m² | 65.0 ft-lb/in² | ASTM D1822 |
ExxonMobil Paxon™ AD60-005 Blow Molding Resin Product Description: AD60-005 is a medium molecular weight districution high-density polyethylene homopolymer. It possesses excellent processing uniformity and produces bottles with excellent appear.. |
|||
Tensile Impact Strength | 137 kJ/m² | 65.0 ft-lb/in² | ASTM D-1822 |
Axiall 3217 Rigid PVC, Extrusion Georgia Gulf 3217 is a powder blend designed for the extrusion of window, door, fence and marine profiles where weatherability is of primary consideration.Information provided by Georgia GulfGeorgia.. |
|||
Tensile Impact Strength | 137 kJ/m² | 65.0 ft-lb/in² | ASTM D-1822 |
Axiall 5006 Rigid PVC, Extrusion, Natural Georgia Gulf 5006 Natural is a rigid PVC pellet compound designed for extrusion of interior rigid PVC profiles and various contours where high gloss and ease of processing is required. Georgia Gulf.. |
|||
Tensile Impact Strength | 137 kJ/m² | 65.0 ft-lb/in² | ASTM D-1822 |
Axiall 5006 Rigid PVC, Extrusion, White Georgia Gulf 5006 White is a rigid PVC pellet compound designed for extrusion of rigid PVC house siding, window profiles and various contours where maximum weather resistance is required. Georgia G.. |