Axiall 3217 Rigid PVC, Extrusion

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 3217 Rigid PVC, Extrusion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Georgia Gulf 3217 is a powder blend designed for the extrusion of window, door, fence and marine profiles where weatherability is of primary consideration.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 88
88
ASTM D-785
Hardness, Shore D 81
81
ASTM D-2240
Tensile Strength, Yield 43.4 MPa
6300 psi
ASTM D-638
Tensile Modulus 2.72 GPa
395 ksi
ASTM D-638
Flexural Strength 89.6 MPa
13000 psi
ASTM D-790
Flexural Modulus 2.96 GPa
430 ksi
ASTM D-790
Izod Impact, Notched 0.801 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
1.50 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D-256
Tensile Impact Strength 137 kJ/m²
65.0 ft-lb/in²
ASTM D-1822
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 66.7 °C
152 °F
ASTM D-648
Processing Properties Metric English Comments
Melt Temperature 193 °C
380 °F
Users viewing this material also viewed the following: