Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.0147 GPa | 2.13 ksi | JIS K6301 |
Stellarchem GP-965B TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
100% Modulus | 0.0147 GPa | 2.13 ksi | |
Taiwan Sheen Soon Sheenthane® A9720 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
100% Modulus | 0.0147 GPa | 2.13 ksi | 500 mm/min; ASTM D 412 |
Zylog Neoplast® 250 FT EB Thermoplastic Vulcanizate Neoplast 250 FT EB is a hard, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding, Blow Molding and Extrusion applications.Ro.. |
|||
100% Modulus | 0.0147 GPa | 2.13 ksi | ASTM D412 |
Elastocon TPE Technologies Elastocon® SMR1000 Thermoplastic Polyolefin Elastomer Elastocon® SMR1000 thermoplastic polyolefin elastomer has been developed for applications that require impact resistance and a high gloss scratch and mar resistant surface finish. Elastocon® SMR10.. |