Taiwan Sheen Soon Sheenthane® A9720 Thermoplastic Polyurethane Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane TPE , Polyurethane, TP
Manufacturer Taiwan Sheen Soon Co. Ltd.
Trade Name Sheenthane®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Taiwan Sheen Soon Sheenthane® A9720 Thermoplastic Polyurethane Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD.
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore A 96 - 100
96 - 100
Tensile Strength 44.1 MPa
6400 psi
Elongation at Break 450 %
450 %
100% Modulus 0.0147 GPa
2.13 ksi
300% Modulus 0.0245 GPa
3.56 ksi
Processing Properties Metric English Comments
Processing Temperature 185 - 210 °C
365 - 410 °F