Mechanical Properties Metric English Comments
100% Modulus 0.0104 GPa
1.51 ksi
ASTM D412-80
DuPont Performance Polymers Hypalon® 20 Chlorosulfonated Polyethylene Rubber, Peroxide Cured Carbon Black Filled Compound
Carbon black compound with 100 parts Hypalon; 40 parts carbon black; 20 parts magnesia; and 5.8 parts Varox® DBPH-50. Physical property data below (except mooney viscosity) are for vulcanizate. Ma..
100% Modulus 0.0104 GPa
1.51 ksi
ASTM D412
Lubrizol ESTANE® ETE50DS3 Ester Based Thermoplastic Polyurethane
Features: Excellent physical and low temperature properties with very good chemical resistance and wide processing window for extrusion.Uses: Flat die/cast film and tubing extrusion and Injection an..
100% Modulus 0.0104 GPa
1.51 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
Dow Nordel® IP 4520 Molded Brake Part
FormulationNordel® IP 4520