Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.0104 GPa | 1.51 ksi | ASTM D412-80 |
DuPont Performance Polymers Hypalon® 20 Chlorosulfonated Polyethylene Rubber, Peroxide Cured Carbon Black Filled Compound Carbon black compound with 100 parts Hypalon; 40 parts carbon black; 20 parts magnesia; and 5.8 parts Varox® DBPH-50. Physical property data below (except mooney viscosity) are for vulcanizate. Ma.. |
|||
100% Modulus | 0.0104 GPa | 1.51 ksi | ASTM D412 |
Lubrizol ESTANE® ETE50DS3 Ester Based Thermoplastic Polyurethane Features: Excellent physical and low temperature properties with very good chemical resistance and wide processing window for extrusion.Uses: Flat die/cast film and tubing extrusion and Injection an.. |
|||
100% Modulus | 0.0104 GPa | 1.51 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4520 Molded Brake Part FormulationNordel® IP 4520 |