Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00950 GPa | 1.38 ksi | ISO/R527 |
Polykemi AB POLYelast TPE S902A Thermoplastic Elastomer, SBS-based Information provided by Polykemi AB |
|||
100% Modulus | 0.00950 GPa | 1.38 ksi | DIN 53504 |
Huntsman IROGRAN® A 92 P 4207 TPU-Polyether Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman |
|||
100% Modulus | 0.00950 GPa | 1.38 ksi | Air aged 14 days at 175°C |
DuPont Vamac® GLS Sample Compound Vulcanizate Slab Cured Test slab is press cured for 5 minutes at 177°C and post cured for 4hrs at 175°C. Vulcanizate performance test data can help end-users evaluate the potential fitness of similar compounds for thei.. |
|||
100% Modulus | 0.00950 GPa | 1.38 ksi | ISO 37 |
Lubrizol ESTANE® 58130 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
100% Modulus | 0.00950 GPa | 1.38 ksi | ISO 37 |
Lubrizol ESTANE® GP92AB Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
100% Modulus | 0.00950 GPa | 1.38 ksi | DIN 53504 |
Lubrizol ESTANE® 58360 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
100% Modulus | 0.00950 GPa | 1.38 ksi | ISO 37 |
ELASTO UK Dryflex® 9012-001 TPE, Modified Injection Molding Grade for Semi Rigid Molding The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. VTC Dryflex® 9012-001 is specifically designe.. |
|||
100% Modulus | 0.00950 GPa | 1.38 ksi | ASTM D1414, ASTM D412 |
DuPont Performance Polymers Kalrez® 9500 Fluoroelastomer DuPont™ Kalrez® 9500 perfluoroelastomer parts are a tan product for Deposition, Ash/Strip and Conductor (Poly/Metal) Etch processes. It has been specifically designed for use in applications where.. |
|||
100% Modulus | 0.00950 GPa | 1.38 ksi | ASTM D412 |
C.O.I.M. LARIPUR® LPR2103-90AE PTMG Polyether Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |